PENGARUH PENAMBAHAN SIKA VISCOCRETE - 10 SEBESAR 1,6 % DAN BUBUK KACA SEBESAR 4 % DARI BERAT SEMEN TERHADAP KUAT TEKAN BETON DAN SLUMP (PENAMBAHAN DILAKUKAN SECARA BERTAHAP SELAMA 60 MENIT)

M. RAHMAT HIDAYAT (2011) PENGARUH PENAMBAHAN SIKA VISCOCRETE - 10 SEBESAR 1,6 % DAN BUBUK KACA SEBESAR 4 % DARI BERAT SEMEN TERHADAP KUAT TEKAN BETON DAN SLUMP (PENAMBAHAN DILAKUKAN SECARA BERTAHAP SELAMA 60 MENIT). S1 thesis, Universitas Muhammadiyah Yogyakarta.

[thumbnail of Halaman Judul] Text (Halaman Judul)
Halaman Judul.pdf

Download (100kB)
[thumbnail of Bab I] Text (Bab I)
Bab I.pdf

Download (44kB)
[thumbnail of Bab II] Text (Bab II)
Bab II.pdf
Restricted to Registered users only

Download (60kB)
[thumbnail of Bab III] Text (Bab III)
Bab III.pdf
Restricted to Registered users only

Download (83kB)
[thumbnail of Bab IV] Text (Bab IV)
Bab IV.pdf
Restricted to Registered users only

Download (148kB)
[thumbnail of Bab V] Text (Bab V)
Bab V.pdf
Restricted to Registered users only

Download (154kB)
[thumbnail of Lampiran] Text (Lampiran)
Lampiran.pdf
Restricted to Repository staff only

Download (106kB)

Abstract

Bubuk kaca atau fritz adalah serpihan kaca yang dihancurkan dan biasa digunakan untuk campuran pembuatan keramik di pabrik keramik. Bubuk kaca mempunyai kandungan SiO2, Al2O3, Fe2O3 dan CaO yang berpotensi untuk digunakan sebagai bahan pengganti semen. Bubuk kaca ini bersifat pozzolan, sehingga bila dipakai sebagai pengganti sebagian semen portland, bahan ini dapat membuat beton lebih tahan terhadap garam, sulfat dan air asam. Sika Viscocrete - 10 adalah bahan tambah kimia Tipe F, yaitu pengura

Item Type: Thesis (S1)
Uncontrolled Keywords: BUBUK KACA, SIKA VISCOCRETE - 10, NILAI KUAT TEKAN, NILAI SLUMP
Divisions: Fakultas Teknik > Teknik Sipil S1
Depositing User: Unnamed user with email robi@umy.ac.id
Date Deposited: 06 Jul 2022 02:30
Last Modified: 06 Jul 2022 02:30
URI: https://etd.umy.ac.id/id/eprint/12235

Actions (login required)

View Item
View Item