KUAT TEKAN BETON METODE ERNTROY DAN SHACKLOCK DENGAN VARIASI FAS 0.28-0,32 UNTUK UKURAN AGREGAT KASAR MAKSIMUM 20 MM

JAFRIANTO (2008) KUAT TEKAN BETON METODE ERNTROY DAN SHACKLOCK DENGAN VARIASI FAS 0.28-0,32 UNTUK UKURAN AGREGAT KASAR MAKSIMUM 20 MM. S1 thesis, Universitas Muhammadiyah Yogyakarta.

[thumbnail of Halaman Judul] Text (Halaman Judul)
Halaman Judul.pdf

Download (158kB)
[thumbnail of Abstract] Text (Abstract)
Abstract.pdf

Download (26kB)
[thumbnail of Bab I] Text (Bab I)
Bab I.pdf

Download (80kB)
[thumbnail of Bab II] Text (Bab II)
Bab II.pdf
Restricted to Registered users only

Download (298kB)
[thumbnail of Bab III] Text (Bab III)
Bab III.pdf
Restricted to Registered users only

Download (92kB)
[thumbnail of Bab IV] Text (Bab IV)
Bab IV.pdf
Restricted to Registered users only

Download (334kB)
[thumbnail of Bab V] Text (Bab V)
Bab V.pdf
Restricted to Registered users only

Download (146kB)
[thumbnail of Bab V] Text (Bab V)
Bab V.pdf
Restricted to Registered users only

Download (45kB)
[thumbnail of Lampiran] Text (Lampiran)
Lampiran.pdf
Restricted to Repository staff only

Download (234kB)

Abstract

Hasil penelitian menunjukan semakin besar faktor air semen maka semakin rendah nilai kuat tekan yang dihasilkan

Item Type: Thesis (S1)
Uncontrolled Keywords: KUAT TEKAN BETON
Divisions: Fakultas Teknik > Teknik Sipil S1
Depositing User: Unnamed user with email robi@umy.ac.id
Date Deposited: 08 Feb 2022 08:54
Last Modified: 08 Feb 2022 08:54
URI: https://etd.umy.ac.id/id/eprint/22285

Actions (login required)

View Item
View Item