KUAT TARIK BELAH CAMPURAN TANAH LEMPUNG DAN SERAT SABUT KELAPA YANG TELAH DIRENDAM DENGAN NAOH PADA BERBAGAI KONSENTRASI

PANDU PERDANA PUTRA (2022) KUAT TARIK BELAH CAMPURAN TANAH LEMPUNG DAN SERAT SABUT KELAPA YANG TELAH DIRENDAM DENGAN NAOH PADA BERBAGAI KONSENTRASI. S1 thesis, Universitas Muhammadiyah Yogyakarta.

[thumbnail of Halaman Judul] Text (Halaman Judul)
Halaman Judul.pdf

Download (392kB)
[thumbnail of Lembar Pengesahan] Text (Lembar Pengesahan)
Lembar Pengesahan.pdf
Restricted to Registered users only

Download (83kB)
[thumbnail of Abstrak] Text (Abstrak)
Abstrak.pdf
Restricted to Registered users only

Download (14kB)
[thumbnail of Bab I] Text (Bab I)
Bab I.pdf

Download (20kB)
[thumbnail of Bab II] Text (Bab II)
Bab II.pdf
Restricted to Registered users only

Download (70kB)
[thumbnail of Bab III] Text (Bab III)
Bab III.pdf
Restricted to Registered users only

Download (785kB)
[thumbnail of Bab IV] Text (Bab IV)
Bab IV.pdf
Restricted to Registered users only

Download (229kB)
[thumbnail of Bab V] Text (Bab V)
Bab V.pdf
Restricted to Registered users only

Download (11kB)
[thumbnail of Daftar Pustaka] Text (Daftar Pustaka)
Daftar Pustaka.pdf
Restricted to Registered users only

Download (78kB)
[thumbnail of Lampiran] Text (Lampiran)
Lampiran.pdf
Restricted to Registered users only

Download (541kB)
[thumbnail of Naskah Publikasi] Text (Naskah Publikasi)
Naskah Publikasi.pdf
Restricted to Registered users only

Download (549kB)
[thumbnail of Full Text] Text (Full Text)
Full Text.pdf
Restricted to Repository staff only

Download (1MB)

Abstract

KEKUATAN TANAH MERUPAKAN SALAH SATU HAL YANG PERLU DIPERHATIKAN DALAM PEKERJAAN DI BIDANG KONSTRUKSI. BEBERAPA JENIS TANAH MEMILIKI DAYA DUKUNG YANG RENDAH SEPERTI TANAH LEMPUNG LUNAK, SEHINGGA DIPERLUKAN ADANYA PERBAIKAN TANAH. SALAH SATU ALTERNATIF BAHAN YANG DAPAT DIGUNAKAN UNTUK PERKUATAN TANAH ADALAH SERAT SABUT KELAPA YANG SUDAH DIRENDAM OLEH CAIRAN NAOH. PENELITIAN INI BERTUJUAN UNTUK MENENTUKAN KONSENTRASI NAOH YANG PALING OPTIMUM AGAR DIPEROLEH NILAI KUAT TARIK BELAH TANAH CAMPURAN YANG MAKSIMUM. PENELITIAN INI MENGGUNAKAN SERAT SABUT KELAPA YANG BERUKURAN 3-5 CM DENGAN KADAR SEBESAR 0,6%. SERAT TERSEBUT DIRENDAM DENGAN CAIRAN NAOH SELAMA 3 JAM TERLEBIH DAHULU DENGAN TUJUAN MEMPERKASAR PERMUKAAN SERAT SABUT KELAPA SEHINGGA DAPAT MENINGKATKAN IKATAN (INTETLOCKING) DENGAN TANAH. PENGUJIAN YANG DILAKUKAN ADALAH PENGUJIAN KUAT TARIK BELAH BERDASARKAN STANDAR SNI-2491. VARIASI YANG DIGUNAKAN ADALAH KADAR NAOH, YAITU SEBESAR 0%, 5%, 10%, 15%, DAN 20%. PADA PENGUJIAN DIGUNAKAN MASING-MASING 3 BENDA UJI PADA SETIAP VARIASINYA. HASIL PENELITIAN INI MENUNJUKKAN BAHWA PERENDAMAN SERAT DENGAN NAOH TIDAK BERPENGARUH TERHADAP NILAI KUAT TARIK BELAH DARI CAMPURAN. DAPAT DILIHAT DARI NILAI YANG PALING MAKSIMAL JUSTRU DIDAPATKAN DARI SAMPEL PENGUJIAN TANAH DENGAN CAMPURAN SERAT YANG TIDAK DIRENDAM NAOH, DIMANA NILAI RATA-RATA KUAT TARIK MAKSIMUMNYA SEBESAR 33,48 KPA.

Item Type: Thesis (S1)
Uncontrolled Keywords: SOFT CLAY, COCONUT FIBER, NAOH, SPLIT TENSILE STRENGTH
Divisions: Fakultas Teknik > Teknik Sipil S1
Depositing User: Eko Kurnawan
Date Deposited: 23 May 2022 03:24
Last Modified: 23 May 2022 03:24
URI: https://etd.umy.ac.id/id/eprint/31837

Actions (login required)

View Item
View Item